News and Media

    24 | 04 | 18
    Marine Alloys: Pick ‘n Mix Technical Workshops
    Marine
    alloys, copper-nickel, corrosion
    Two leading trade associations have combined forces to offer tailored in-house technical workshops to those needing to better understand the behaviour of copper-based alloys, stainless steels and nickel alloys in marine environments.
    01 | 06 | 17
    Strong Corrosion Performance of Copper Alloys Highlighted at Marine Conference
    Marine
    alloys, corrosion, marine
    CDA will make an invited presentation—Metals in Marine Environments: Corrosion Behaviour and How to Spot It—to the International Institute of Marine Surveying at this year’s Seawork International Show and Conference, with a focus on the strong contribution copper alloys can make to marine engineering.
    22 | 02 | 17
    Copper Alloys: State-of-the-Art Engineering on the Agenda at Corrosion 2017
    Marine
    corrosion
    The development of copper alloys—from traditional applications to state-of-the-art engineering—will be described in a symposium at NACE International’s Corrosion 2017.
    07 | 03 | 16
    Copper Alloys in Seawater: New Publication Launched
    Marine
    engineer, corrosion, marine, copper-nickel
    A new technical publication has launched this week at NACE’s Corrosion 2016: ‘Copper Alloys in Seawater: Avoidance of Corrosion Problems’, by Roger Francis.
    03 | 02 | 16
    Knowledge Exchange on Copper Alloys at Corrosion 2016
    Marine
    alloys, copper-nickel, corrosion, marine
    Copper Alliance will be exhibiting at Booth 539 of NACE International’s Corrosion 2016 – offering information and knowledge exchange on copper alloys – and participating in Technical Exchange Group TEG 523X Marine Corrosion of Copper Alloys.
    27 | 01 | 16
    Engineers’ Guide to Nickel Aluminium Bronze Launched
    Marine
    marine, offshore, engineer, corrosion, bronze, applications, alloys
    A new publication offers practical guidance for engineers wishing to specify, design or produce nickel aluminium bronze components for marine, aerospace and other sectors.