Copper-iron-phosphorus-magnesium

Copper-iron-phosphorus-magnesium CuFePMg

Copper-iron-phosphorus-magnesium is a heat treatable copper-iron alloy with small additions of magnesium. It is stronger and harder than pure copper with slightly lower electrical conductivity.

Go to Quick Facts

 

History

Since the 1930s, copper has been alloyed with small amounts of magnesium as a lower cost alternative to silver. These alloys, developed in the USA, aim to increase the strength of copper particularly at temperatures up to 300oC, whilst maintaining a high electrical conductivity.

In 1980, the Olin Corporation USA developed a copper-iron-magnesium alloy specifically for electronic applications such as lead frames. The alloy, magnesium content 0.1 to 1.0%, is heat treatable and its properties depend on the formation of tiny (less than 0.5 micron) precipitates.

Further developments in the metallurgy of this alloy type continued with a Japanese alloy produced in 2004 with small additions of nickel, cobalt and zinc which after heat treatment, resulted in precipitates of 0.2 microns leading to improved strength, formability and conductivity.

Heat Treatment

The precipitation heat treatment involves heating the alloy to 800 to 900oC and water quenching. This is called solution treatment and the alloy is in its softest condition.

Subsequent precipitation (age) hardening at lower temperatures of 425 to 500oC, results in the formation of finely dispersed precipitates which are responsible for the increased strength, formability and hardness.

Properties

The alloy has a combination of the following properties as below:

  • Tensile strength: 296-552 N/mm2
  • 0.2% Proof strength: 110-490 N/mm2
  • % Elongation: 15-2
  • Hardness (HV): 122-190
  • Electrical conductivity: 80% IACS
  • Thermal conductivity: 277-320 W/moC

Stress Relaxation

This is a decrease in stress under constant strain, typically observed in bolts in turbine casings at high temperatures, which must be regularly tightened.

With copper alloys used for electrical/electronic components, it is important to maintain good contact force throughout the functional life of the product and have good resistance to stress relaxation.

One indication of stress relaxation resistance may be obtained by measuring the % of stress which is retained as a function of temperature and time.

Results on test pieces for this alloy show that 70% of the applied stress (80% of proof stress) remained after 1000 hours at 150oC. This is useful information in the design of contacts, connectors, springs, relays and lead frames.

Fabrication

Process Rating
Cold formability Good
Hot formability Good
Soldering Excellent
Brazing Good
Oxyacetylene welding Fair
Gas shield arc welding Good
Resistance welding Good

Machining

Machinability rating is 20% which is adequate. Free-machining brass is 100%.

Resistance to Corrosion

The alloy has good resistance to corrosion in industrial and marine atmospheres. It is insensitive to stress corrosion cracking. However, it is susceptible to attack in the presence of ammonia, sulphur, hydrogen sulphide and mercury.

Resistance to Softening

Tests have shown that this alloy may be used for short periods up to 350oC without softening. A hardness of 180 HV was maintained for one hour at this temperature.

Applications

This alloy is suited to applications which require excellent formability, high strength and electrical and thermal conductivity, together with excellent corrosion resistance and solderability.

  • Lead frames
  • Fuse clips
  • Connectors
  • Circuit breaker components

Available Forms

CuFePMg is available as bar, plate, rod, sheet and strip.

Specifications

Below is the specification for US. For equivalent standards from other countries visit the Copper Key website.

  • USA: C19700 (American Society for Testing and Materials ASTM designation)

Further information on C19700 and other conductivity materials, is available at the Copper Alloys Knowledge Base.

Application Example 1: Fuse Clips

A fuse clip supports a fuse and provides electrical connection with it. The high strength, stiffness and electrical conductivity make this alloy ideal for this application.

Fuse clip
Fuse clip (Courtesy of Standard Electric Supply Co).

Application Example 2: Circuit Breaker Components

The high strength at temperature, high hardness and good conductivity make this alloy ideal for this application. The principle is to create a zero current condition within a few milliseconds.

Details of this circuit breaker are to be found in CDA Publication 223: Copper in Electrical Contacts. 

Sequence of events
Sequence of events in an arc quenching arrangement in a typical miniature circuit breaker. Click for a larger view. Details of this circuit breaker are to be found in CDA Publication 223: Copper in Electrical Contacts.

Quick Facts

Properties
The alloy has the following combination of properties:

  • Tensile strength: 296-552 N/mm2
  • 0.2% Proof strength: 110-490 N/mm2
  • % Elongation: 15-2
  • Hardness (HV): 122-190
  • Electrical conductivity: 80% IACS
  • Thermal conductivity: 277-320 W/moC

Applications

  • Lead frames
  • Fuse clips
  • Connectors
  • Circuit breaker components

Available Forms

  • Bar
  • Plate
  • Rod
  • Sheet
  • Strip

This section lists coppers and copper alloys for conductivity applications. The alloys are grouped by property. Individual alloy pages include details of specifications, mechanical and physical properties, available product forms and applications

For equivalents of copper alloys worldwide, their chemical compositions, material designation and national standards

Visit the Copper Alloys Knowledge Base for detailed technical information