Your download will start shortly

pub-41-clear-protective-coatings-for-copper-pdf.pdf    |    579 KB

Click the button below if the download doesn't start in 3 seconds

Download manually

Pub 041 – Clear Protective Coatings for Copper and Copper Alloys

Detailed description of the range of coatings available with application methods and recommendations for use. 1991. 24pp.