Pub 117 – The Brasses – Properties and Applications

This publication provides information on compositions and properties of standard brasses (including nickel-silvers) in wrought and cast condition, together with details of BS and European Standards, forms available, fabrication methods and examples of typical applications. 2005. 64pp.