Pub071 - The Nickel-silvers

Nickel silvers are silver/white coloured copper alloys with varying additions of zinc and nickel. This publication gives information on mechanical properties, typical applications, joining techniques, heat treatment, fabrication, surface finishing. 1965. 27pp.

Download document